PAGE 2 OF 2 |
|
2.2.3 |
MAXIMUM THERMAL CONDUCTIVITY:
The thermal conductivity shall not exceed the following
for any density:
BTU in./h Ft2°F (W/m K)
|
Mean Temperature
|
0.33 (0.048) |
200°F (93°C) |
0.43 (0.062)
|
300°F (149°C)
|
0.54 (0.078)
|
400°F (204°C)
|
|
|
2.2.4 |
MAXIMUM NON-FIBROUS (SHOT) CONTENT:
The percentage content of non-fibrous material (shot) shall
not exceed 20% by weight (ASTM C1335) |
| |
2.2.5 |
WATER VAPOR SORPTION:
The water vapor sorption shall be less than 1% by weight. |
| |
2.2.6 |
STRESS CORROSION:
The material must not promote or contribute to the corrosion
of austenitic stainless steel. |
| |
2.2.7 |
SURFACE BURNING CHARACTERISTICS:
Shall not exceed
Flame Spread 5 Smoke Developed 0 |
| |
2.2.8 |
NOISE REDUCTION COEFFICIENT:
The NRC shall not be less than 0.95 |
APPROVED MANUFACTURE (S): FIBREX INSULATIONS,
INC. or equal
Single or multiple layer -
FBX INDUSTRIAL BOARD
FBX INDUSTRIAL FLEXIBLE BATT
|
3. |
INSTALLATION
Recommended industry standards, similar to those listed in
the MICA manual, are to be followed.
NATIONAL COMMERCIAL AND INDUSTRIAL INSULATION STANDARDS
Produced By:
MIDWEST INSULATION CONTRACTORS ASSOCIATION
2017 SOUTH 139TH. CIRCLE
OMAHA, NE 68144
Phone: (402) 342-3463
Fax: (402) 330-9702 |
4. |
STANDARDS AND TEST METHODS
ASTM C 612, CAN/CGSB-51.10-92 |
INDUSTRIAL BOARD INSULATION STANDARD |
ASTM C 553, CAN/CGSB-51.11-M |
INDUSTRIAL FLEXIBLE BATT STANDARD |
ASTM E 84, CAN4-S102, UL 723 |
SURFACE BURNING CHARACTERISTICS |
ASTM E 136, CAN4-S114 |
NON-COMBUSTIBILITY |
ASTM C 177 |
THERMAL CONDUCTIVITY |
ASTM C 303 |
DENSITY |
ASTM C 356 |
LINEAR SHRINKAGE |
ASTM C 411 |
HOT SURFACE PERFORMANCE |
ASTM C 447 |
ESTIMATING MAXIMUM USE TEMPERATURE |
ASTM C 795 |
INSULATION FOR USE OVER AUSTENITIC STAINLESS
STEEL |
ASTM C 871 |
CHEMICAL ANALYSIS |
NRC 1.36 |
STRESS CORROSION AND CHEMICAL ANALYSIS |
ASTM C 423, E 795 |
SOUND ABSORPTION |
|